Handling adhesive area on inner door panel
WARNING: This page is about a different variant/trim than selected.
| Adhesive |
Cleaning |
- Butyl bead applied to sound insulation with protective film
- Butyl mini-round profile Ø 3 mm from the roller
- Butyl round profile Ø 6 mm from the roller
|
- CLEANING AGENTR2
Under no circumstances: paint thinning
- Carry out bonding only after an air drying time ≥ 1 min. Air drying time may be omitted if the entire bonding surface is wiped with a dry cloth
- After cleaning, the bonding surface may not be touched with hands or fouled again
|