LEMON Manuals: Even more car manuals for everyone
Home >> Porsche >> 2016 >> Macan Turbo >> Repair and Diagnosis >> External Pages >> Different car >> Section 107 (46 - Brakes - Brake Mechanics -- PANAMERA (970)) >> WM 465102 Checking Front PCCB Brake Discs (Wear Assessment) (Except PANAMERA GTS, PANAMERA Turbo S, PANAMERA 4 Executive, PANAMERA Platinum Ed., PANAMERA 4 Platinum Ed.) >> Checking PCCB Brake Discs (Wear Assessment) >> Evaluation Of Surface Roughness Rk (Max. 80 Micrometers Permitted)

Evaluation Of Surface Roughness Rk (Max. 80 Micrometers Permitted)

WARNING: This page does not describe the selected car, but rather 7 other vehicles, including the 2016 Porsche Panamera, 2015 Porsche Panamera, 2014 Porsche Panamera, 2013 Porsche Panamera, and 2012 Porsche Panamera. However, it is still accessible from the selected car via links, so may be relevant.

Information 

The assessment is carried out visually, based on the diagram. Two illustrations of the same peak-to valley surface roughness (views 1 and 2) help to make a better assessment.

  1. Brake discs that are OK: 
    1. 1.1. Surface roughness Rk = 6 μm - see-  (Fig 1 )
      Fig 1: Identifying PCCB Surface Roughness (Rk) = 6 Micrometers (View 1)
      G09808038Courtesy of PORSCHE CARS NORTH AMERICA, INC.

      Surface roughness Rk = 6 μm -see-  (Fig 2 )

      New brake disc. Illustration is used for better classification.

      The early stages of roughness are indicated by burnt-out carbon fibres on the surface of an otherwise intact, semi-matt surface.

      The surface feels smooth.

      Fig 2: Identifying PCCB Surface Roughness (Rk) = 6 Micrometers (View 2)
      G09808039Courtesy of PORSCHE CARS NORTH AMERICA, INC.
    2. 1.2. Surface roughness Rk = 56 μm -see-  (Fig 3 )
      Fig 3: Identifying PCCB Surface Roughness (Rk) = 56 Micrometers (View 1)
      G09808040Courtesy of PORSCHE CARS NORTH AMERICA, INC.

      Surface roughness Rk = 56 μm -see-  (Fig 4 )

      In the advanced stages of fibre burnout and the initial destruction of the Si and SiC 'matrix', the depressions have become more pronounced. Large sections of the surface are still intact, the depressions form an even, fine-grained pattern.

      The surface still feels matt, however, and the roughness is not yet pronounced.

      No replacement necessary!

      Fig 4: Identifying PCCB Surface Roughness (Rk) = 56 Micrometers (View 2)
      G09808041Courtesy of PORSCHE CARS NORTH AMERICA, INC.
    3. 1.3. Surface roughness Rk = 72 μm -see-  (Fig 5 )
      Fig 5: Identifying PCCB Surface Roughness (Rk) = 72 Micrometers (View 1)
      G09808042Courtesy of PORSCHE CARS NORTH AMERICA, INC.

      Surface roughness Rk = 72 μm -see-  (Fig 6 )

      Borderline disc, which can still just be evaluated as OK. As a result of more advanced damage to the surface, the depressions are larger, and above all deeper, compared with the previous surface condition.

      On the one hand, the more extensive roughness is noticeable (only when a comparison is made); on the other hand, however, like before, "only" depressions are observed.

      Replacement not yet necessary!

      Fig 6: Identifying PCCB Surface Roughness (Rk) = 72 Micrometers (View 2)
      G09808043Courtesy of PORSCHE CARS NORTH AMERICA, INC.
  2. Worn brake discs: 
    1. 2.1. Surface roughness Rk = 108 μm -see-  (Fig 7 )
      Fig 7: Identifying PCCB Surface Roughness (Rk) = 108 Micrometers (View 1)
      G09808044Courtesy of PORSCHE CARS NORTH AMERICA, INC.

      Surface roughness Rk = 108 μm -see-  (Fig 8 )

      Worn surface. Advanced wear has led to a situation where only the remains of the original surface are left.

      It is clear that the roughness is caused not only by depressions but also by bumps.

      Replace brake discs! To do this, follow the instructions → 465102 CHECKING FRONT PCCB BRAKE DISC (WEAR ASSESSMENT) .

      In general, the following applies: Brake discs must be replaced if the surface roughness (Rk) is > 80 μm!

      Fig 8: Identifying PCCB Surface Roughness (Rk) = 108 Micrometers (View 2)
      G09808045Courtesy of PORSCHE CARS NORTH AMERICA, INC.
  3. Worn brake discs (special cases): 
    1. 3.1. Surface roughness Rk = 108 μm, as for previous disc, but with some of the original friction surface remaining -arrow-  .

      Replace brake discs! To do this, follow the instructions → 465102 CHECKING FRONT PCCB BRAKE DISC (WEAR ASSESSMENT) .

      In general, the following applies: Brake discs must be replaced if the surface roughness (Rk) is > 80 μm!

      Fig 9: Identifying PCCB Surface Roughness (Rk) = 108 Micrometers
      G09808046Courtesy of PORSCHE CARS NORTH AMERICA, INC.
    2. 3.2. Surface roughness Rk = 72 μm. Borderline brake disc detected based on roughness, as well as wear indication and connected surface fractures -arrows-  , > 1 cm2 .

      Replace brake discs! To do this, follow the instructions → 465102 CHECKING FRONT PCCB BRAKE DISC (WEAR ASSESSMENT) .

      Fig 10: Locating PCCB Brake Disc
      G09808047Courtesy of PORSCHE CARS NORTH AMERICA, INC.