Home >> Mini >> 2014 >> Cooper Base, 2D Convertible, Automatic Trans >> Repair and Diagnosis >> External Pages >> Different car >> Section 3036 (COLLISION - BODY PANEL REPAIR (E90) 328i, 328xi, 335i, 335xi) >> 4100 Body Panel Repair General Information >> 4100... Information On Metal Filler >> Processing

4100... Information On Metal Filler: Processing

WARNING: This page does not describe the selected car, but rather 10 other vehicles, including the 2011 BMW 328xi, 2011 BMW 328i, 2010 BMW 335xi, 2010 BMW 335i, and 2010 BMW 328xi. However, it is still accessible from the selected car via links, so may be relevant.

The working temperature of the metal filler must be at least 18°C.

Fig 1: Identifying Metal Filler And Hardener
G06854677Courtesy of BMW OF NORTH AMERICA, INC.

A = Metal filler

B = Hardener

NOTE: The mixture ratio refers to the volume.

Mix metal filler in mixture ratio of 5:2. Mix components thoroughly and free of pores.

IMPORTANT: Do not stir components. Danger of air pockets in metal filler!

Working life of the metal filler is approx. 45 minutes.