Hardening Time

WARNING: This page does not describe the selected car, but rather 6 other vehicles, including the 2010 BMW 535xi, 2010 BMW 535i, 2009 BMW 535xi, 2009 BMW 535i, and 2008 BMW 535xi. However, it is still accessible from the selected car via links, so may be relevant.

The metal filler must be hardened using a short-wave infrared heater.

IMPORTANT: In the first 10 minutes, the temperature of 50°C may not be exceeded. In contrast, a temperature that is too low may be equalized by extending the time.
NOTE: When the heater is used for the first time, the distances that match the temperature must be determined.

Switch the heater on and change the distance until the surface temperature of the metal filler no longer changes for a period of 2 minutes. Measure the temperature with a temperature gauge. When optical temperature gauges are used (Epsilon value 0.92-0.95), the heater must be switched off briefly during the measurement. Record the measurement