Home >> Mini >> 2010 >> Cooper S, 2D Hatchback, Standard >> Repair and Diagnosis >> External Pages >> Different car >> Section 1177 (Collision - Body Panel Repair (E92 & E93)) >> Body Panel Repair General Information >> 41 00... Straightening Aluminum Components In Structure >> Reshaping Or Heating Extruded Sections And Cast Parts Is Not Permitted

Reshaping Or Heating Extruded Sections And Cast Parts Is Not Permitted

WARNING: This page does not describe the selected car, but rather 21 other vehicles, including the 2013 BMW 328xi, 2013 BMW 328i, 2012 BMW 328xi, 2012 BMW 328i, and 2011 BMW 328xi. However, it is still accessible from the selected car via links, so may be relevant.

Failure to comply with this requirement would have the following results:

In the case of reshaping, weld seams (E52) or glued connections (E60, E61, E63, E64) tear in the surrounding area.

In the case of reshaping, the material loses up to 40 % of its original strength.

In the case of heating, the material loses up to 40 % of its original strength.

The adhesive is destroyed at temperatures =120°C (E60, E61, E63, E64).

Extruded sections and cast parts which show visible or measurable signs of deformation must be replaced.

Perform the check for deformation with the aid of the straightening system.

For optical testing, strip adjoining components in cases of doubt.

Extruded sections are used in the E52 as engine supports, door pillars, side members, etc.

Extruded sections are used in the E60, E61, E63, E64 as engine supports.

Cast parts are used in the E60, E61, E63, E64, E70, E71 as spring supports.