General information
WARNING: This page does not describe the selected car, but rather 6 other vehicles, including the 2015 BMW 760Li, 2014 BMW 760Li, 2013 BMW 760Li, 2012 BMW 760Li, and 2011 BMW 760Li. However, it is still accessible from the selected car via links, so may be relevant.
- The following procedures are used for repairs:
- MAG welding (M etal Ac tive G as welding)
- Resistance pressure spot welding (referred to in the following and in the repair instructions as spot welding).
- Take the number and location of weld spots and MAG weld seams from the separated part. Replace areas inaccessible to spot-welding tongs with MAG plug/spot welds at the same distance. Diameter of bores for plug/spot welds 8 mm.
- In the case of emissions extraction, observe a minimum distance of 30 cm for MAG welding during the welding process. Otherwise the inert gas would be drawn off.
- Follow the equipment manufacturer's instructions for use.