Prepare Mating Surfaces On Vehicle For Center Roof Paneling - Ar65.10-P-1000-08FRC

Model 290 with code 397 (Carbon roof) 

IMPORTANT Further information is available in the superordinate service document.

The safety information in the superordinate service document must be observed.

G16555513Courtesy of MERCEDES-BENZ USA

NOTES Do not touch hatched areas with bare fingers. Keep free from dust, oil, grease, wax, dirt residues, and other adhesive components.

The strength of the adhesively bonded connection is otherwise impaired and the required adhesion of the adhesive material is not ensured.

NOTES Only use materials from window repair kit approved and always observe processing notes included.

The strength of the adhesively bonded connection is otherwise impaired and the required adhesion of the adhesive material is not ensured.

NOTES If new parts were installed in the area of the carbon roof frame during a body repair, mask off bonding surfaces before painting.

The strength of the adhesively bonded connection is otherwise impaired and the required adhesion of the adhesive material is not ensured.

NOTES Ensure that adhesive material is applied only to present adhesive beads, which have been cut down, or to the original factory primer or repair primer approved by Daimler.

The strength of the adhesively bonded connection is otherwise impaired and the required adhesion of the adhesive material is not ensured.

Prepare body flange for panoramic roof 

  1. Cut back residual adhesive material on the body flange to a maximum remaining height of 1 mm.
  2. Remove cut off adhesive material residues from the body flange.
  3. Repair paint damage on body flange.

    IMPORTANT Use only primers and paints approved by Daimler AG: https://portal.aftersales.i.daimler.com

  4. Apply primer in gluing area if glue residues are not present.

    NOTES Observe processing notes for primer. Comply with flash-off time of at least 10 min.

    Otherwise, there will be adhesion problems with the adhesive material when gluing in the carbon roof.

    NOTES Apply primer only after primer has dried.

    The strength of the adhesively bonded connection is otherwise impaired and the required adhesion of the adhesive material is not ensured.