LEMON Manuals: Even more car manuals for everyone
Home >> Mercedes Benz >> 1995 >> E420 >> Repair and Diagnosis >> External Pages >> Different car >> Section 28 (Electrical System, Equipment & Instructions - 140 Chassis) >> Repair & Adjustments >> Treatment of battery when the car is laid up - ra54001400006x(0006)

Treatment of battery when the car is laid up - ra54001400006x(0006)

WARNING: This page does not describe the selected car, but rather 42 other vehicles, including the 1999 Mercedes-Benz S600, 1999 Mercedes-Benz S500, 1999 Mercedes-Benz S420, 1999 Mercedes-Benz S320, and 1999 Mercedes-Benz CL600. However, it is still accessible from the selected car via links, so may be relevant.

Model 140 

Preliminary work:

Charge battery, check state of charge and capacity, A (Charging, checking the state and capacity of the battery  ).

Operation no. of operation texts and work units or standard texts and flat rates:

IMPORTANT Observe warning information and safety regulations (Initial filling of the battery  , A).

Retract trunk lid handle by actuating switch on trunk lock.

Fig 1: Identifying Trunk Lock
G05439010Courtesy of MERCEDES-BENZ OF NORTH AMERICA.
NOTE: As of approx. 01/95 the switch on the trunk lock has been eliminated. In this case it is necessary to retract the trunk lid grip manually with the lever (1) and switch off the closing assist with the switch (2). Lock vehicle manually or with infrared remote control.
Fig 2: Identifying Lever And Switch
G05439011Courtesy of MERCEDES-BENZ OF NORTH AMERICA.

IMPORTANT The pin in the trunk lid auxiliary lock should not be extended, if necessary repeat locking procedure.

Fig 3: Identifying Trunk Lid Auxiliary Lock
G05439012Courtesy of MERCEDES-BENZ OF NORTH AMERICA.
  1. Disconnect ground cable from battery.
  2. Recharge battery every three months and then measure electrolyte density.

Electrolyte density specification  1.28 kg/dm3 (see table).

Never allow the battery to stand discharged, otherwise sulfate will deposit on the plates. Sulfated  plates damage the battery leading to premature failure.

Anti-freeze protection  as function of state of charge

State of charge in kg/dm3 at 20 °C Electrolyte density Normal solidification temperature of electrolyte in °C
charged 1.28 - 65
semi-charged 1.20 - 30
discharged 1.12 - 4
NOTE: The electrolyte density is dependent on the temperature and varies by 0.01 kg/dm3 for each 15 °C.

Examples:

Electrolyte density at 20 °C 1.28 kg/dm3

Electrolyte density at 35 °C 1.29 kg/dm3

Electrolyte density at 5 °C 1.27 kg/dm3

COMMERCIALLY AVAILABLE TESTER

Acidimeter e. g. Hazet