3.2 Application
At 20... 25 °C the mix can be processed after approx. 5... 10 minutes (pot time).
Apply thin (approx. 0.5 mm), uniform coat of glue on base with spatula and press base onto glass in such a way that glue obtains good contact with windshield across the entire surface area.
NOTE:
The temperature for the hardening process should not be lower than +18 °C.