3. Preparations For Brazing Solder And Tinning
WARNING: This page is about a different variant/trim than selected.
- Heat brazed connections to be opened with gas flame. Lift off sheet metal remnants and remove remaining brazing solder with wire brush.
- Remove the paint and zinc layer in an area of approx. 30 mm around the seam to be soldered.
- Remove the paint and zinc layer in the tin-plating area and approx. 30 mm beyond.