1. General Information
WARNING: This page is about a different variant/trim than selected.
- The following procedures are used for repairs:
- MAG welding (M etal A ctive G as welding)
- Resistance pressure spot welding (referred to in the following and in the repair instructions as spot welding).
- Take the number and position of welding spots and MAG weld seams from the separated part. Replace areas inaccessible to spot-welding tongs with MAG plug weldings at the same distance. Diameter of bore holes for plug weldings 8 mm.
- In the case of emissions extraction, observe a minimum distance of 30 cm for MAG welding during the welding process. Otherwise the inert gas would be drawn off.
- Follow the equipment manufacturer's instructions for use.